Temperature dependent reflectance measurements at 25 °C, 60 °C, and 100 °C are illustrated in Fig. 7a,b. It could be observed that the VO2 skinny films exhibit a significant rate of transform of reflectance upon heating, which correlated with previous report by Guinneton et al.A electronic area is particularly essential for stronger prescrip